|本期目录/Table of Contents|

[1]王江浩,耿 欧,李富民.再生粗骨料多种改性方法对混凝土抗压强度提升效果的试验[J].建筑科学与工程学报,2016,33(02):91-97.
 WANG Jiang-hao,GENG Ou,LI Fu-min.Experiment on Effect of Several Measures by Modifying Recycled Coarse Aggregate on Improving Compressive Strength of Concrete[J].Journal of Architecture and Civil Engineering,2016,33(02):91-97.
点击复制

再生粗骨料多种改性方法对混凝土抗压强度提升效果的试验(PDF)
分享到:

《建筑科学与工程学报》[ISSN:1673-2049/CN:61-1442/TU]

卷:
33卷
期数:
2016年02期
页码:
91-97
栏目:
出版日期:
2016-03-30

文章信息/Info

Title:
Experiment on Effect of Several Measures by Modifying Recycled Coarse Aggregate on Improving Compressive Strength of Concrete
作者:
王江浩耿 欧李富民
中国矿业大学江苏省土木工程环境灾变与结构可靠性重点实验室
Author(s):
WANG Jiang-hao, GENG Ou, LI Fu-min
Jiangsu Key Laboratory of Environmental Impact and Structural Safety in Engineering, China University of Mining and Technology
关键词:
废弃混凝土再生粗骨料改性抗压强度
Keywords:
waste concrete recycled coarse aggregate modification compressive strength
分类号:
-
DOI:
-
文献标志码:
A
摘要:
为对比粗骨料多种改性方法对混凝土抗压强度的提升效果,分别采用不同质量分数的盐酸溶液和8%质量分数草酸溶液以及25%质量分数防水砂浆浆液和2%质量分数聚乙烯醇浆液对再生粗骨料进行化学浸洗或物理填充,将处理得到的再生粗骨料制成边长为100 mm的立方体混凝土试件进行抗压强度测试。结果表明:粗骨料的不同处理方式对混凝土抗压强度均有不同程度的提高,其中2%质量分数盐酸溶液(处理效果接近最佳)、8%质量分数草酸溶液、25%质量分数防水砂浆浆液和2%质量分数聚乙烯醇浆液处理骨料分别可使混凝土抗压强度提高11.84%,7%,4.37%,11.31%,并达到同级配天然碎石骨料混凝土抗压强度的96.63%,92.44%,90.18%,96.17%。
Abstract:
In order to compare the effect of several measures by modifying recycled coarse aggregate on improving compressive strength of concrete, the HCl solution with different concentrations, H2C2O4 solution with concentration of 8%, waterproofing mortar solution with concentration of 25% and PVA solution with concentration of 2% were used to treat the recycled coarse aggregate samples by chemical immersion or physical filling, respectively. By using the treated recycled coarse aggregate,some cubic concrete samples with the dimension of 100 mm×100 mm×100 mm were fabricated for testing the compressive strength. The results show that different treatments may achieve an increase in the compressive strength of the mixed concrete to some different extents. Comparing with the untreated recycled coarse aggregate, the aggregates treated respectively with the above-mentioned HCl solution with concentration of 2% (closing to the best effect), H2C2O4 solution with concentration of 8%, waterproofing mortar solution with concentration of 25%, and PVA solution with concentration of 2% contribute to an increase in the compressive strength of the mixed concrete for 11.84%, 7%, 4.37% and 11.31%, respectively. The increased compressive strength achieves a good level as high as 96.63%, 92.44%, 90.18% and 96.17% of the concrete mixed with the natural coarse aggregate, which has the same grain composition with the recycled coarse aggregate.

参考文献/References:

相似文献/References:

[1]肖建庄,范玉辉.再生混凝土徐变试验及机理的模型化分析[J].建筑科学与工程学报,2012,29(04):18.
 XIAO Jian-zhuang,FAN Yu-hui.Experiment and Mechanism Modeling Analysis on Creep of Recycled Aggregate Concrete[J].Journal of Architecture and Civil Engineering,2012,29(02):18.
[2]肖建庄,马旭伟,刘 琼,等.全再生混凝土概念的衍化与研究进展[J].建筑科学与工程学报,2021,38(02):1.[doi:10.19815/j.jace.2020.11036]
 XIAO Jian-zhuang,MA Xu-wei,LIU Qiong,et al.Evolvement and Research Progress of Concept for Full Recycled Concrete[J].Journal of Architecture and Civil Engineering,2021,38(02):1.[doi:10.19815/j.jace.2020.11036]
[3]陈旭勇,艾阳正,程书凯,等.再生粗骨料性能指标分布及相关性分析[J].建筑科学与工程学报,2023,40(02):1.[doi:10.19815/j.jace.2021.10082]
 CHEN Xuyong,AI Yangzheng,CHENG Shukai,et al.Performance indexes distribution and correlation analysis of recycled coarse aggregate[J].Journal of Architecture and Civil Engineering,2023,40(02):1.[doi:10.19815/j.jace.2021.10082]

备注/Memo

备注/Memo:
更新日期/Last Update: 2016-03-30